Applying a waterproofing coating to the interior surface of a concrete block foundation is a standard practice in foundation waterproofing, yet homeowners often question if the same treatment can be effectively applied to the exterior face of a masonry veneer, specifically brick. The question of using a drylok on brick surfaces arises frequently during exterior renovations and new construction, where the desire for a finished look clashes with the need for moisture management. This situation creates a dilemma: how does one achieve a sealed, painted appearance without compromising the structural integrity of the wall system or violating fundamental installation principles.

Understanding the Core Function of Drylok

Drylok is a brand-specific term that has entered the common lexicon to describe a specific type of cementitious waterproofing paint. Unlike standard exterior paints that sit on top of a substrate, these products are designed to be integrated into the surface they cover. The active mechanism relies on crystalline growth, where additives within the mixture react with water and cement to form insoluble crystals that penetrate deep into the pores of the masonry.
This chemical reaction effectively blocks water vapor and liquid water from passing through the material, transforming a permeable surface into a waterproof barrier. It is specifically engineered for use on concrete, cinder block, stone, and stucco, where capillary action can draw moisture inward. The primary goal is to prevent water intrusion that leads to efflorescence, spalling, and structural damage within the wall cavity.

The Incompatibility of Direct Application on Brick
While the product is highly effective on solid concrete, applying a drylok on brick is generally not recommended and violates standard construction practices. Brick veneer is not a solid monolithic wall; it is a facade attached to a drainage plane with an air gap behind it. This cavity is essential for allowing moisture that penetrates the outer skin to drain back to the exterior without entering the living space.

Sealing the porous surface of the brick with a drylok coating traps the moisture within the masonry unit and the mortar joints. Instead of allowing the wall to dry to the exterior, the water becomes suspended, leading to a variety of detrimental issues. This includes freeze-thaw damage, where water expansion cracks the brick or spalls the surface, and prolonged dampness that promotes mold growth within the wall assembly.
Mortar Joints and Surface Texture
The physical properties of brick and mortar create another barrier to application. Mortar joints are typically compressed during the tooling process, creating a dense, slick surface that does not bond well with cementitious coatings. Furthermore, the rough, irregular texture of extruded brick faces provides a mechanical key that standard drywall or concrete substrates possess.

When a drylok is applied over a smooth, non-porous mortar bed, the coating can peel off in sheets. The adhesion relies on the porous nature of the substrate; when that porous substrate is absent, the film lacks the necessary grip to remain intact, resulting in premature failure and a messy appearance that detracts from the curb appeal of the home.
Addressing Efflorescence and Moisture Issues
Homeowners often turn to drylok as a solution to visible efflorescence, the white powdery residue that appears on brick surfaces. This residue indicates that soluble salts are being pushed to the surface by internal water pressure. While the product can mask this issue temporarily by creating a film, it does not address the root cause of the moisture problem.

If the water pressure is high enough to push salts through the brick, it will also push through the drylok coating. This often results in the blistering and peeling of the paint as the water vapor seeks an exit point. Proper treatment involves identifying the source of the moisture—whether it is a failing flashing, poor grading, or hydrostatic pressure—and correcting it before any cosmetic finish is considered.
Correct Alternatives for Finished Brick Exteriors


















For those seeking a smooth, painted finish on a brick exterior, there are appropriate methods that respect the behavior of the material. The most effective approach is to clean the brick thoroughly to remove efflorescence and dirt, then install a breathable masonry water repellent. These treatments are designed to bead water on the surface while allowing vapor to escape, preserving the breathability of the wall.
Once the substrate is treated and sealed with the appropriate clear sealer, a high-quality exterior masonry paint can be applied. These paints are formulated to flex with the natural movement of the brick and mortar, providing the desired color and protection without trapping moisture within the wall cavity. This method ensures longevity and maintains the structural integrity of the drainage plane.
Summary and Best Practices
Understanding the specific function of a product is crucial before applying it to a structural component. Drylok serves a vital purpose in protecting solid foundation walls from groundwater intrusion, but its application logic does not translate to veneer brick systems. The risks of trapping moisture and causing hidden damage far outweigh the aesthetic benefit of a sealed surface.
Homeowners and contractors should prioritize moisture management and breathability when dealing with brick exteriors. By utilizing the correct water repellents and masonry paints, it is possible to achieve a clean, uniform appearance while ensuring the wall assembly remains healthy and durable for decades. Respecting the materials and their installation guidelines is the best path to a successful and lasting finish.