Covering a brick wall with mortar is a foundational technique in both new construction and renovation, transforming a rough, uneven surface into a primed canvas for plaster, tile, or paint. This process, known as repointing or skimming, involves applying a thin layer of mortar to create a smooth, stable, and aesthetically pleasing finish. Success hinges on meticulous surface preparation, the correct mortar mix, and a disciplined application process, ensuring the new layer bonds securely and lasts for decades.
Understanding the Purpose and Scope
The primary goal of applying a mortar layer over existing brick is to correct imperfections, improve thermal performance, or provide a clean base for finishing materials. This is distinct from repointing, which focuses on replacing degraded mortar in the joints between bricks. When skimming a wall, you are essentially creating a new outer skin, typically ranging from 3 to 12 millimeters thick. It is crucial to determine the exact scope of your project—is the entire wall unstable, or are you only addressing specific damaged areas? Understanding this will dictate the preparation required and the type of mortar you select.
Critical Surface Preparation
No step is more vital to the success of mortar application than preparing the brick substrate. Mortar will not bond effectively to a dirty, dusty, or smooth surface. The brick must be thoroughly cleaned using a stiff wire brush to remove soot, algae, and old paint flakes. Any loose or crumbling mortar joints must be chiseled out to a depth of at least 10 millimeters to create a solid anchor point. For maximum adhesion, consider washing the wall with a pressure washer or a mild acid solution, followed by a complete rinse and an extended drying period. The bricks must be absolutely sound and saturated with water (but not wet) before the mortar is applied to prevent the base material from robbing the water from your new skim coat.

Selecting the Right Mortar Mix
The choice of mortar is dictated by the function of the finished wall and the local climate. For a basic skim coat intended to receive paint, a standard cement mortar mix is usually sufficient. However, if the wall will be exposed to significant moisture, such as in a basement or outdoor setting, a polymer-modified mortar or a lime-based mix is highly recommended due to its superior flexibility and breathability. The mortar must be workable enough to be spread evenly yet strong enough to cure without cracking. Always follow the manufacturer's instructions regarding the water-to-mix ratio, and never add extra water to the applied batch to make it more workable, as this weakens the final structure.
Step-by-Step Application Process
Applying the mortar requires patience and attention to detail to achieve a uniform finish.
- Begin by installing a vertical screed board at the top of the wall to define the thickness of the mortar layer.
- Using a suitable hawk and trowel, scoop a manageable amount of mortar onto the board.
- Spread the mortar across the wall in a sweeping motion, ensuring full coverage of the brick surface.
- Immediately use the edge of the trowel to press the mortar firmly into the brick texture, creating a key bond.
- Once the wall is covered, use a slightly damp sponge or a wood float to gently level the surface and remove high spots.
- Allow the layer to "set up" slightly, then use a wood trowel to apply the final smooth finish, depending on whether you prefer a textured dash finish or a sleek, polished look.
Curing and Protection
The curing phase is just as critical as the application. If the mortar dries too quickly, it will shrink and crack. To prevent this, the wall must be kept moist. Mist the surface with water regularly for at least 48 to 72 hours, particularly during hot or windy weather. Protect the newly applied mortar from direct sunlight, freezing temperatures, and physical impact. Curing is not complete until the mortar has reached its full strength, which can take up to 28 days, so avoid washing or treating the wall harshly during this period.

Troubleshooting Common Issues
Even with careful preparation, issues can arise. "Blowing" occurs when the mortar detaches from the brick, usually due to poor bonding or contamination on the surface. "Cracking" is often the result of improper curing or using a mix that is too wet. "Efflorescence," the white, powdery salt deposits that appear on the surface, happens when water evaporates and leaves behind salts from the mortar or brick. Addressing these problems requires removing the compromised mortar, thoroughly cleaning the area, and reapplying a corrected mortar mix with strict attention to the curing process.