Concrete Kerb Repair
The following section describes a failure sequence of a 480mm deep kerb. The crack begins at Point A and spreads predominantly downwards. When the tensile strength exceeds the strength of the concrete, the front concrete haunch separates from the concrete base. Although the force is mostly in tension, there is some flexure as the front concrete haunch separates from the base concrete.